To catalogue
Starflam™ AFR200Y
- Chemical Family
- Polyamides
Starflam AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66 Injection Molding Resin
Properties
- Physical Form
- Pellets
- Solid
Product families
Plastics — Engineering & Specialty Polymers
- Polyamides
Other characteristics
- Brand
- Starflam
- Polymer Name
- Polyamide 66 (PA 66)
- Flexural Modulus
- 3300.0 - 3300.0 MPa
- Additives Included
- Flame Retardant
- Processing Methods
- Extrusion, Injection Molding
- Color
- Custom
- Flame Rating
- UL 94 V0
- Technology
- Plastics
- Labeling Claims
- Halogen-free
- Material Features
- Flame Retardant
- Low Odor
- Low Phosphorus Content
- Country Availability
- Brazil
- Canada
- China (Mainland)
- Mexico
- USA
- Certifications and Compliance
- UL 94
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 5
14 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Stress at break | 78 | MPa | ISO 527 |
| Tensile Modulus | 3400 | MPa | ISO 527 |
| Yield stress | 80 | MPa | ISO 527 |
| Yield strain | 4.8 | % | ISO 527 |
| Strain at break | 9 | % | ISO 527 |
| Flexural modulus, 23° | 3300 | MPa | ISO 178 |
| Charpy notched impact strength (+23°) | 3 | kJ/m2 | ISO 179/1eA |
| Charpy notched impact strength (-30°) | 3 | kJ/m2 | ISO 179/1eA |
| Charpy impact strength (+23°) | 100 | kJ/m2 | ISO 179/1eU |
| Charpy impact strength (-30°) | 70 | kJ/m2 | ISO 179/1eU |
| Izod notched impact strength, +23° | 4 | kJ/m2 | ISO 180/1A |
| Izod notched impact strength | 3 | kJ/m2 | ISO 180/1A |
Table 2 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1170 | kg/m3 | ASTM D 792 |
Table 3 of 5
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Coefficient of Linear Thermal Expansion (parallel) | 85 | E-6/K | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 85 | E-6/K | ISO 11359-1/-2 |
| Temperature of deflection under load (1.80 Mpa) | 90 | °C | ISO 75-1/-2 |
| Temperature of deflection under load (0.45 Mpa) | 210 | °C | ISO 75-1/-2 |
| Oxygen index | 29 | % | ISO 4589-1/-2 |
| Thickness tested | 0.75 | mm | — |
| Vicat softening temperature | 247 | °C | ISO 306 |
Table 4 of 5
1 row| Characteristic | Value | Method |
|---|---|---|
| Flame rating | V-0 | UL 94 |
Table 5 of 5
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water absorption | 7.5 | % | Sim. to ISO 62 |
| Humidity absorption | 1.1 | % | Sim. to ISO 62 |