To catalogue
Staramide™ AK8
- Chemical Family
- Polyamides
Staramide AK8 is a 40 % Mineral Filled Polyamide 66 Injection Molding Resin
Properties
- Physical Form
- Pellets
- Solid
Product families
Plastics — Engineering & Specialty Polymers
- Polyamides
Other characteristics
- Brand
- Staramide
- Polymer Name
- Polyamide 66 (PA 66)
- Fillers Included
- Mineral
- Flexural Modulus
- 5200.0 - 5200.0 MPa
- Processing Methods
- Extrusion, Injection Molding
- Color
- Custom
- Technology
- Plastics
- Material Features
- Low Odor
- Country Availability
- Brazil
- Canada
- China (Mainland)
- Mexico
- USA
- Certifications and Compliance
- ISO 14001
- ISO 9001
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Extrusion
- Injection Molding
Technical data
Table 1 of 4
12 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Stress at break | 75 | MPa | ISO 527 |
| Tensile Modulus | 5200 | MPa | ISO 527 |
| Strain at break | 10 | % | ISO 527 |
| Flexural modulus, 23° | 5200 | MPa | ISO 178 |
| Charpy notched impact strength (+23°) | 7 | kJ/m2 | ISO 179/1eA |
| Charpy impact strength (+23°) | 100 | kJ/m2 | ISO 179/1eU |
| Charpy notched impact strength (-30°) | 6 | kJ/m2 | ISO 179/1eA |
| Charpy impact strength (-30°) | 100 | kJ/m2 | ISO 179/1eU |
| Izod notched impact strength, +23° | 7 | kJ/m2 | ISO 180/1A |
| Izod notched impact strength | 7 | kJ/m2 | ISO 180/1A |
| Rockwell Hardness | 92 | Scale L | ISO 2039-2 |
| Temperature | -30 | °C | — |
Table 2 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1450 | kg/m3 | ASTM D 792 |
Table 3 of 4
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Coefficient of Linear Thermal Expansion (parallel) | 60 | E-6/K | ISO 11359-1/-2 |
| Coefficient of Linear Thermal Expansion (normal) | 60 | E-6/K | ISO 11359-1/-2 |
| Temperature of deflection under load (1.80 Mpa) | 170 | °C | ISO 75-1/-2 |
| Temperature of deflection under load (0.45 Mpa) | 231 | °C | ISO 75-1/-2 |
| Oxygen index | 32 | % | ISO 4589-1/-2 |
| Vicat softening temperature | 252 | °C | ISO 306 |
Table 4 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Humidity absorption | 0.9 | % | Sim. to ISO 62 |