To catalogue

Polymer Resources Ltd. PRL PEI-G10

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
  • Consumer Electronics
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies

Product Families

Plastics — Engineering & Specialty Polymers
  • High Performance Thermoplastics

Other characteristics

Polymer Name
Polyether Imide (PEI)
Fillers Included
Glass Fiber
Processing Methods
Injection Molding
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Additives
Flame Retardant
Features
  • Flame Retardant
  • High Heat Resistance
Availability
North America
Technology
Plastics
Processing Method
Injection Molding
Quality Standards
UL Yellow Card (E113219)
Material Features
  • Flame Retardant
  • Heat Resistance
  • UL Flame Rated
Country Availability
  • Canada
  • Mexico
  • USA
Filler/Reinforcement
Filler
Glass Fiber
Reinforcement
10% Filler by Weight
Agency Ratings
RoHS Compliant
Certifications and Compliance
RoHS Compliant
Plastics and Elastomers End Uses
  • Appliances
  • Medical Devices
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 8

6 rows
CharacteristicValueUnitMethod
Density1.34—ASTM D792
Melt Mass Flow Rate (at 337°C, 6.6 kg)5.0 - 22g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)4.0E-3 to 6.0E-3in/inASTM D955
Water Absorption (24 hrs)0.21%ASTM D570
Water Absorption (at Equilibrium, 73°F)1.2%ASTM D570
Specific Gravity1.34—ASTM D792

Table 2 of 8

6 rows
CharacteristicValueUnitMethod
Tensile Modulus (at 0.125 in)660000psiASTM D638
Tensile Strength (at Yield, 0.125 in)16500psiASTM D638
Tensile Strength (at Break, 0.125 in)16500psiASTM D638
Tensile Elongation (at Break, 0.125 in)6%ASTM D638
Flexural Modulus (at 0.125 in)740000psiASTM D790
Flexural Strength (at 0.125 in)27000psiASTM D790

Table 3 of 8

10 rows
CharacteristicValueUnitMethod
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)405°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)400°FASTM D648
Coefficient of Linear Thermal Expansion (at -4 to 302°F, Flow)1.8e-05in/in/°FASTM E831
Relative Thermal Index Electrical Property (at 0.06 in)221°FUL 746
Relative Thermal Index Electrical Property (at 0.12 in)221°FUL 746
Relative Thermal Index Impact Property (at 0.06 in)221°FUL 746
Relative Thermal Index Impact Property (at 0.12 in)221°FUL 746
Relative Thermal Index Strength Property (at 0.06 in)221°FUL 746
Relative Thermal Index Strength Property (at 0.12 in)221°FUL 746
Vicat Softening Temperature430°FASTM D1525 ²

Table 4 of 8

5 rows
CharacteristicValueUnitMethod
Volume Resistivity1.0e+17ohms·cmASTM D257
Dielectric Strength (at 0.0625 in, in Oil)690V/milASTM D149
Dielectric Constant (at 1 kHz)3.5—ASTM D150
Dissipation Factor (at 1 kHz)0.0014—ASTM D150
Dissipation Factor (at 2 GHz)0.0046—ASTM D150

Table 5 of 8

2 rows
CharacteristicValueMethod
Flame Rating (at 0.06 in, All)V-0UL 94
Flame Rating (at 0.12 in, All)V-0UL 94

Table 6 of 8

8 rows
CharacteristicValueUnit
Drying Temperature290 - 300°F
Drying Time4.0 - 6.0hr
Front Temperature650 - 750°F
Middle Temperature640 - 750°F
Mold Temperature225 - 350°F
Rear Temperature630 - 750°F
Maximum Drying Time24hr
Processing Temperature (Melt)640 - 750°F

Table 7 of 8

3 rows
CharacteristicValueUnitMethod
Impact Strength (at 73°F, 0.125 in, Notched Izod)1ft·lb/inASTM D256
Impact Strength (at 73°F, 0.125 in, Unnotched Izod)9ft·lb/inASTM D4812
Impact Strength (at 73°F, 0.125 in, Reverse Notch Izod)7.5ft·lb/inASTM D256

Table 8 of 8

1 row
CharacteristicValueMethod
Rockwell Hardness (M-Scale)114ASTM D785

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.