To catalogue

Polymer Resources Ltd. PRL PC/ASA-GP2

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
  • Consumer Electronics
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies

Product Families

Plastics — Engineering & Specialty Polymers
  • Blends & Alloys

Other characteristics

Density
1140.0 - 1140.0 kg/m³
Polymer Name
PC/ASA Alloy
Processing Methods
Injection Molding
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Features
  • General Purpose
  • Medium Flow
  • Medium Impact Resistance
Availability
North America
Technology
Plastics
Processing Method
Injection Molding
Material Features
  • Good Flow
  • Impact Resistance
Country Availability
  • Canada
  • Mexico
  • USA
Agency Ratings
RoHS Compliant
Certifications and Compliance
RoHS Compliant
Plastics and Elastomers End Uses
  • Appliances
  • General Purpose
  • Lenses
  • Medical Devices
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 5

4 rows
CharacteristicValueUnitMethod
Density1.14—ASTM D792
Melt Mass Flow Rate (at 220°C, 10 kg)8.0 - 18g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)5.0E-3 to 7.0E-3in/inASTM D955
Specific Gravity1.14—ASTM D792

Table 2 of 5

4 rows
CharacteristicValueUnitMethod
Tensile Strength (at Yield, 0.125 in)8500psiASTM D638
Tensile Strength (at Break, 0.125 in)7500psiASTM D638
Flexural Modulus (at 0.125 in)377000psiASTM D790
Flexural Strength (at 0.125 in)11000psiASTM D790

Table 3 of 5

2 rows
CharacteristicValueUnitMethod
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)215°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)190°FASTM D648

Table 4 of 5

8 rows
CharacteristicValueUnit
Drying Temperature190 - 210°F
Drying Time3.0 - 4.0hr
Front Temperature490 - 520°F
Middle Temperature470 - 490°F
Mold Temperature130 - 160°F
Maximum Drying Time8hr
Rear Temperature450 - 470°F
Processing Temperature (Melt)490 - 520°F

Table 5 of 5

2 rows
CharacteristicValueUnitMethod
Impact Strength (at 73°F, 0.125 in, Notched Izod)8ft·lb/inASTM D256
Gardner Impact Strength (at 0.125 in)min. 320in·lbASTM D3029

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.