To catalogue
Polymer Resources Ltd. PRL NY66-GP2
- Chemical Family
- Polyamides
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Applications
- Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
- Consumer Electronics
Healthcare & Pharma — Medical
- Medical Devices & Assemblies
Product Families
Plastics — Engineering & Specialty Polymers
- Polyamides
Other characteristics
- Polymer Name
- Polyamide 66 (PA 66)
- Additives Included
- Lubricant (Unspecified), Nucleating Agent
- Lubricant (Unspecified)
- Nucleating Agent
- Processing Methods
- Injection Molding
- Usage
- General Purpose
- Markets
- Consumer Goods
- Electrical & Electronics
- Healthcare & Pharma
- Additives
- Lubricant
- Nucleating Agent
- Features
- General Purpose
- Lubricated
- Nucleated
- Availability
- North America
- Technology
- Plastics
- Processing Method
- Injection Molding
- Material Features
- Lubricated
- Nucleated
- Country Availability
- Canada
- Mexico
- USA
- Agency Ratings
- RoHS Compliant
- Certifications and Compliance
- RoHS Compliant
- Plastics and Elastomers End Uses
- Appliances
- General Purpose
- Medical Devices
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 6
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1.14 | — | ASTM D792 |
| Molding Shrinkage (at 0.125 in, Flow) | 0.012 - 0.018 | in/in | ASTM D955 |
| Molding Shrinkage (at 0.125 in, Across Flow) | 0.015 - 0.021 | in/in | ASTM D955 |
| Specific Gravity | 1.14 | — | ASTM D792 |
Table 2 of 6
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus (at 0.125 in) | 490000 | psi | ASTM D638 |
| Tensile Strength (at Yield, 0.125 in) | 13000 | psi | ASTM D638 |
| Tensile Strength (at Break, 0.125 in) | 13000 | psi | ASTM D638 |
| Tensile Strain (at Yield, 0.125 in) | 4.5 | % | ASTM D638 |
| Tensile Strain (at Break, 0.125 in) | 30 | % | ASTM D638 |
| Flexural Modulus (at 0.125 in) | 440000 | psi | ASTM D790 |
| Flexural Strength (at 0.125 in) | 17000 | psi | ASTM D790 |
Table 3 of 6
2 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed) | 475 | °F | ASTM D648 |
| Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed) | 215 | °F | ASTM D648 |
Table 4 of 6
8 rows| Characteristic | Value | Unit |
|---|---|---|
| Drying Temperature | 165 - 185 | °F |
| Drying Time | 3.0 - 4.0 | hr |
| Front Temperature | 530 - 550 | °F |
| Middle Temperature | 520 - 540 | °F |
| Mold Temperature | 150 - 200 | °F |
| Rear Temperature | 510 - 530 | °F |
| Maximum Drying Time | 8 | hr |
| Processing Temperature (Melt) | 530 - 560 | °F |
Table 5 of 6
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Impact Strength (at -22°F, Notched Charpy) | 1.8 | ft·lb/in² | ISO 179/1eA |
| Impact Strength (at 73°F, Notched Charpy) | 2 | ft·lb/in² | ISO 179/1eA |
| Impact Strength (at 73°F, 0.125 in, Notched Izod) | 1 | ft·lb/in | ASTM D256 |
| Impact Strength (at 73°F, Notched Izod) | 1.5 | ft·lb/in² | ISO 180/1A |
Table 6 of 6
1 row| Characteristic | Value | Method |
|---|---|---|
| Rockwell Hardness (R-Scale) | 120 | ASTM D785 |