To catalogue

Polymer Resources Ltd. PRL ABS-G25

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
  • Consumer Electronics
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies

Product Families

Plastics — Basic Thermoplastics
  • Styrenics

Other characteristics

Polymer Name
Acrylonitrile Butadiene Styrene (ABS)
Fillers Included
Glass Fiber
Processing Methods
Injection Molding
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Availability
North America
Technology
Plastics
Processing Method
Injection Molding
Material Features
Easier Processing
Country Availability
  • Canada
  • Mexico
  • USA
Filler/Reinforcement
Filler
Glass Fiber
Reinforcement
25% Filler by Weight
Agency Ratings
RoHS Compliant
Certifications and Compliance
RoHS Compliant
Plastics and Elastomers End Uses
  • Appliances
  • Medical Devices
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 5

4 rows
CharacteristicValueUnitMethod
Density1.23—ASTM D792
Melt Mass Flow Rate (at 230°C, 3.8 kg)0.50 - 5.0g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)1.0E-3 to 3.0E-3in/inASTM D955
Specific Gravity1.23—ASTM D792

Table 2 of 5

5 rows
CharacteristicValueUnitMethod
Tensile Strength (at Yield, 0.125 in)13500psiASTM D638
Tensile Strength (at Break, 0.125 in)13500psiASTM D638
Tensile Elongation (at Yield, 0.125 in)1.5%ASTM D638
Flexural Modulus (at 0.125 in)1100000psiASTM D790
Flexural Strength (at 0.125 in)18500psiASTM D790

Table 3 of 5

2 rows
CharacteristicValueUnitMethod
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)230°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)220°FASTM D648

Table 4 of 5

8 rows
CharacteristicValueUnit
Drying Temperature175 - 185°F
Drying Time3.0 - 4.0hr
Front Temperature410 - 440°F
Middle Temperature410 - 430°F
Mold Temperature120 - 160°F
Maximum Drying Time8hr
Rear Temperature380 - 410°F
Processing Temperature (Melt)410 - 460°F

Table 5 of 5

1 row
CharacteristicValueUnitMethod
Impact Strength (at 73°F, 0.125 in, Notched Izod)1ft·lb/inASTM D256

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.