To catalogue

Polymer Resources Ltd. PRL PC/TP-GP3-G30

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
  • Consumer Electronics
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies

Product Families

Plastics — Engineering & Specialty Polymers
  • Blends & Alloys
Composite Materials — Polymers & Resins
  • Thermoplastic Resins

Other characteristics

Density
1440.0 - 1440.0 kg/m³
Polymer Name
PC/Polyester Alloy
Processing Methods
Injection Molding
Reinforcement Material
Glass Fibers
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Additives
Impact Modifier
Features
Chemical Resistant
Availability
North America
Technology
  • Composite Materials
  • Plastics
Fillers Included
Glass Fiber
Processing Method
Injection Molding
Additives Included
Impact Modifier
Material Features
Chemical Resistant
Country Availability
  • Canada
  • Mexico
  • USA
Filler/Reinforcement
Filler
Glass Fiber
Reinforcement
30% Filler by Weight
Agency Ratings
RoHS Compliant
Certifications and Compliance
RoHS Compliant
Composite Materials Functions
Resins Binders & Matrix Materials
Composites Processing Methods
Injection Molding
Plastics and Elastomers End Uses
  • Appliances
  • Lenses
  • Medical Devices
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 5

4 rows
CharacteristicValueUnitMethod
Density1.44—ASTM D792
Melt Mass Flow Rate (at 265°C, 2.16 kg)1.0 - 8.0g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)4.0E-3 to 6.0E-3in/inASTM D955
Specific Gravity1.44—ASTM D792

Table 2 of 5

4 rows
CharacteristicValueUnitMethod
Tensile Strength (at Yield, 0.125 in)13000psiASTM D638
Tensile Strength (at Break, 0.125 in)13000psiASTM D638
Flexural Modulus (at 0.125 in)775000psiASTM D790
Flexural Strength (at 0.125 in)19500psiASTM D790

Table 3 of 5

2 rows
CharacteristicValueUnitMethod
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)390°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)290°FASTM D648

Table 4 of 5

8 rows
CharacteristicValueUnit
Drying Temperature225 - 235°F
Drying Time4.0 - 6.0hr
Front Temperature500 - 540°F
Middle Temperature490 - 530°F
Mold Temperature150 - 200°F
Maximum Drying Time8hr
Rear Temperature480 - 520°F
Processing Temperature (Melt)500 - 550°F

Table 5 of 5

1 row
CharacteristicValueUnitMethod
Impact Strength (at 0.125 in, Notched Izod)2.7ft·lb/inASTM D256