To catalogue
Polymer Resources Ltd. PRL PEI-G30
Properties
- Physical Form
- Pellets
- Solid
Product families
Applications
Applications
- Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
- Consumer Electronics
Healthcare & Pharma — Medical
- Medical Devices & Assemblies
Product Families
Plastics — Engineering & Specialty Polymers
- High Performance Thermoplastics
Other characteristics
- Polymer Name
- Polyether Imide (PEI)
- Fillers Included
- Glass Fiber
- Processing Methods
- Injection Molding
- Markets
- Consumer Goods
- Electrical & Electronics
- Healthcare & Pharma
- Additives
- Flame Retardant
- Features
- Flame Retardant
- High Heat Resistance
- Availability
- North America
- Technology
- Plastics
- Processing Method
- Injection Molding
- Quality Standards
- UL Yellow Card (E113219)
- Material Features
- Flame Retardant
- Heat Resistance
- UL Flame Rated
- Country Availability
- Canada
- Mexico
- USA
- Filler/Reinforcement
- Filler
- Glass Fiber
- Reinforcement
- 30% Filler by Weight
- Agency Ratings
- RoHS Compliant
- Certifications and Compliance
- RoHS Compliant
- Plastics and Elastomers End Uses
- Appliances
- Medical Devices
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 8
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1.51 | — | ASTM D792 |
| Melt Mass Flow Rate (at 337°C, 6.6 kg) | 5.0 - 22 | g/10 min | ASTM D1238 |
| Molding Shrinkage (Flow) | 1.0E-3 to 4.0E-3 | in/in | ASTM D955 |
| Water Absorption (24 hrs) | 0.16 | % | ASTM D570 |
| Water Absorption (at Equilibrium, 73°F) | 0.9 | % | ASTM D570 |
| Specific Gravity | 1.51 | — | ASTM D792 |
Table 2 of 8
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus (at 0.125 in) | 1350000 | psi | ASTM D638 |
| Tensile Strength (at Yield, 0.125 in) | 23500 | psi | ASTM D638 |
| Tensile Strength (at Break, 0.125 in) | 23500 | psi | ASTM D638 |
| Tensile Elongation (at Break, 0.125 in) | 3 | % | ASTM D638 |
| Flexural Modulus (at 0.125 in) | 1290000 | psi | ASTM D790 |
| Flexural Strength (at 0.125 in) | 32000 | psi | ASTM D790 |
Table 3 of 8
11 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed) | 412 | °F | ASTM D648 |
| Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed) | 410 | °F | ASTM D648 |
| Coefficient of Linear Thermal Expansion (at -4 to 302°F, Flow) | 1.0e-05 | in/in/°F | ASTM E831 |
| Coefficient of Linear Thermal Expansion (at -4 to 302°F, Transverse) | 2.3e-05 | in/in/°F | ASTM E831 |
| Relative Thermal Index Electrical Property (at 0.06 in) | 221 | °F | UL 746 |
| Relative Thermal Index Electrical Property (at 0.12 in) | 221 | °F | UL 746 |
| Relative Thermal Index Impact Property (at 0.06 in) | 221 | °F | UL 746 |
| Relative Thermal Index Impact Property (at 0.12 in) | 221 | °F | UL 746 |
| Relative Thermal Index Strength Property (at 0.06 in) | 221 | °F | UL 746 |
| Relative Thermal Index Strength Property (at 0.12 in) | 221 | °F | UL 746 |
| Vicat Softening Temperature | 440 | °F | ASTM D1525 ² |
Table 4 of 8
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Volume Resistivity | 30000000000000000 | ohms·cm | ASTM D257 |
| Dielectric Strength (at 0.0625 in, in Air) | 620 | V/mil | ASTM D149 |
| Dielectric Strength (at 0.0625 in, in Oil) | 760 | V/mil | ASTM D149 |
| Dielectric Constant (at 1 kHz) | 3.7 | — | ASTM D150 |
| Dissipation Factor (at 1 kHz) | 0.0015 | — | ASTM D150 |
| Dissipation Factor (at 2 GHz) | 0.0053 | — | ASTM D150 |
Table 5 of 8
2 rows| Characteristic | Value | Method |
|---|---|---|
| Flame Rating (at 0.06 in, All) | V-0 | UL 94 |
| Flame Rating (at 0.12 in, All) | V-0 | UL 94 |
Table 6 of 8
10 rows| Characteristic | Value | Unit |
|---|---|---|
| Drying Temperature | 290 - 300 | °F |
| Drying Time | 4.0 - 6.0 | hr |
| Front Temperature | 650 - 750 | °F |
| Middle Temperature | 640 - 750 | °F |
| Mold Temperature | 225 - 350 | °F |
| Rear Temperature | 630 - 750 | °F |
| Suggested Shot Size | 40 - 60 | % |
| Maximum Drying Time | 8 | hr |
| Suggested Maximum Moisture Content | 0.02 | % |
| Processing Temperature (Melt) | 640 - 750 | °F |
Table 7 of 8
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Impact Strength (at 73°F, 0.125 in, Notched Izod) | 1.5 | ft·lb/in | ASTM D256 |
| Impact Strength (at 73°F, 0.125 in, Unnotched Izod) | 8 | ft·lb/in | ASTM D4812 |
| Impact Strength (at 73°F, 0.125 in, Reverse Notch Izod) | 8.7 | ft·lb/in | ASTM D256 |
Table 8 of 8
1 row| Characteristic | Value | Method |
|---|---|---|
| Rockwell Hardness | 114 | ASTM D785 |