To catalogue

Polymer Resources Ltd. PRL ABS-GP-HH

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Consumer Goods — Appliances & Electronics
Electrical & Electronics — Devices & Assemblies
  • Consumer Electronics
Healthcare & Pharma — Medical
  • Medical Devices & Assemblies

Product Families

Plastics — Basic Thermoplastics
  • Styrenics

Other characteristics

Polymer Name
Acrylonitrile Butadiene Styrene (ABS)
Processing Methods
Injection Molding
Markets
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Features
  • General Purpose
  • High Heat Resistance
Availability
North America
Technology
Plastics
Processing Method
Injection Molding
Material Features
  • Easier Processing
  • Heat Resistance
Country Availability
  • Canada
  • Mexico
  • USA
Agency Ratings
RoHS Compliant
Certifications and Compliance
RoHS Compliant
Plastics and Elastomers End Uses
  • Appliances
  • General Purpose
  • Medical Devices
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 6

4 rows
CharacteristicValueUnitMethod
Density1.05—ASTM D792
Melt Mass Flow Rate (at 230°C, 3.8 kg)1.0 - 5.0g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)5.0E-3 to 7.0E-3in/inASTM D955
Specific Gravity1.05—ASTM D792

Table 2 of 6

7 rows
CharacteristicValueUnitMethod
Tensile Modulus (at 0.125 in)320000psiASTM D638
Tensile Strength (at Yield, 0.125 in)6500psiASTM D638
Tensile Strength (at Break, 0.125 in)6100psiASTM D638
Tensile Elongation (at Yield, 0.125 in)4.5%ASTM D638
Tensile Elongation (at Break, 0.125 in)25%ASTM D638
Flexural Modulus (at 0.125 in)360000psiASTM D790
Flexural Strength (at 0.125 in)11500psiASTM D790

Table 3 of 6

3 rows
CharacteristicValueUnitMethod
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)215°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)195°FASTM D648
Vicat Softening Temperature240°FASTM D1525 ²

Table 4 of 6

8 rows
CharacteristicValueUnit
Drying Temperature180 - 200°F
Drying Time2.0 - 5.0hr
Front Temperature440 - 490°F
Middle Temperature420 - 460°F
Mold Temperature120 - 180°F
Rear Temperature380 - 410°F
Maximum Drying Time8hr
Processing Temperature (Melt)450 - 525°F

Table 5 of 6

6 rows
CharacteristicValueUnitMethod
Impact Strength (at 73°F, Notched Charpy)5ft·lb/in²ISO 179
Impact Strength (at -40°F, 0.125 in, Notched Izod)1ft·lb/inASTM D256
Impact Strength (at 73°F, 0.125 in, Notched Izod)3.5ft·lb/inASTM D256
Impact Strength (at -40°F, Notched Izod)3ft·lb/in²ISO 180/1A
Impact Strength (at 73°F, Notched Izod)6.2ft·lb/in²ISO 180/1A
Gardner Impact Strength (at 0.125 in)200in·lbASTM D3029

Table 6 of 6

1 row
CharacteristicValueMethod
Rockwell Hardness (R-Scale)112ASTM D785