To catalogue

Techtron® HPV PPS

Techtron® HPV PPS is a high-performance polymer that combines the excellent chemical and corrosion resistance of Polyphenylene Sulfide (PPS) with the added wear resistance and strength of glass fiber reinforcement and internal lubrication. This compression-molded material is designed to excel in demanding environments and applications where wear resistance and dimensional stability are required.Key features:Superior wear resistance: internally lubricated and glass fiber-reinforced, allowing it to withstand high loads and minimize wear and tearOutstanding chemical and hydrolysis resistance: suitable for use in harsh environments and chemicalsExcellent dimensional stability: minimal moisture absorption and low coefficient of linear thermal expansion, making it easy to maintain tight tolerancesGreat electrical insulating and dielectric propertiesLow coefficient of friction and inherent low flammabilityGlass fiber reinforced: increased strength and stiffness, ideal for wear componentsFood grade availableBenefits:Improved performance and durability of components in demanding environmentsIncreased resistance to chemicals, corrosion, and wearEnhanced precision and dimensional stabilityImproved electrical insulation and dielectric propertiesReduced friction and lower flammability riskMore cost-effective than advanced engineering plastics for certain applicationsApplications:Wear components such as bushings and bearings, CIP wash down parts, and pump, valve, and compressor applications in the aerospace, food processing, and oil and gas industries.Industrial equipment such as industrial drying and food processing ovens (bearings, rollers, etc.)Chemical process equipment (pump-, valve & compressor components)Electrical insulating systemsCost-effective alternative to advanced engineering plastics in certain applicationsTechtron® HPV is a versatile and reliable material that can help improve the performance and longevity of your products. It's available in a range of shapes and sizes, including food grade, making it easy to incorporate into your designs.

Properties

Physical Form
  • Plates, Rods
  • Plates
  • Rods

Other characteristics

Brand
Techtron® PPS
Density
1,420.0 kg/m³
Features

Chemical Resistant, Dimensional Stability, Electrically Insulating, Excellent Dielectric Properties, Excellent Hydrolysis Resistance, Food Contact Acceptable, High Tolerance, Low Coefficient of Friction, Low Flammability, Lubricated, Odorless, Wear Resistant

Polymer Name
Polyphenylene Sulfide (PPS)
Tensile Modulus
4,000.0 MPa
Color (Properties)
Blue
Markets
  • Automotive & Transportation
  • Industrial
Flame Rating
UL 94 V0
Technology
Plastics
Labeling Claims
  • Food Contact Acceptable
  • Odor-free
Fillers Included
Glass Fiber
Product Families
Plastics — Parts, Shapes & Films
Engineering Notes

All Mitsubishi Chemical Advanced Materials-EPP's PPS products offer dimensional stability and strength at moderate temperatures. They are rated for continuous service to 425°F (220°C), but strength and stiffness vary based on temperature and grade. Unreinforced Techtron® PPS is generally not recommended for wear applications. Products like Torlon® PAI or Ketron® PEEK are better selections for high temperature wear applications. When designing with compression molded grades, it is important to note its relatively low elongation and impact strength.

Additives Included
Lubricant (Unspecified)
Color
Blue
Material Features
  • Chemical Resistant
  • Dimensional Stability
  • Electrically Insulating
  • Excellent Dielectric Properties
  • Excellent Hydrolysis Resistance
  • Food Contact Acceptable
  • High Tolerance
  • Low Coefficient of Friction
Chemical Inventories
  • TSCA (USA)
  • TSCA Exempt (USA)
Certifications and Compliance
  • FDA Compliant
  • UL 94
Plastics and Elastomers End Uses
  • Aerospace Applications
  • Bearings
  • Bushings
  • Oil/Gas Applications
  • Pump Parts
  • Valves

Technical data

Table 1 of 4

8 rows
CharacteristicValueUnitMethod
Tensile Strength78MPaISO 527-1/-2 (7)
Tensile Strain (Elongation) at Break3.5%ISO 527-1/-2 (7)
Tensile Modulus of Elasticity4000MPaISO 527-1/-2 (9)
Compressive Stress (1 / 2 / 5 % Nominal Strain)33/ 65/105MPaISO 604 (10)
Charpy Impact Strength (Unnotched)25kJ/m²ISO 179-1/1eU
Charpy Impact Strength (Notched)4kJ/m²ISO 179-1/1eA
Flexural Strength118MPaISO 178 (12)
Hardness (14)82Rockwell MISO 2039-2

Table 2 of 4

10 rows
CharacteristicValueUnitMethod
Melting Temperature (DSC, 10°C (50°F) / min)280°CISO 11357-1/-3
Thermal Conductivity (23°C)0.3W/(K.m)—
Coefficient of Linear Thermal Expansion (23 - 60°C)50µm/(m.K)—
Coefficient of Linear Thermal Expansion (23 - 100°C)60µm/(m.K)—
Coefficient of Linear Thermal Expansion (min. 150°C)100µm/(m.K)—
Heat Deflection Temperature (Method A: 1.8 MPa (264 PSI))115°CISO 75-1/-2
Continuous Allowable Service Temperature in Air (20.000 hrs) (3)220°C—
Minimum Service Temperature (4)-20°C—
Flammability (3 mm) (5)V-0—UL 94
Flammability (Oxygen Index)44%ISO 4589-1/-2

Table 3 of 4

5 rows
CharacteristicValueUnitMethod
Electric Strength24kV/mmIEC 60243-1 (15)
Volume Resistivity100000000000000Ohm.cmIEC 62631-3-1
Surface Resistivity10000000000000Ohm/sq.ANSI/ESD STM 11.11
Dielectric Constant (1 MHz)3.3—IEC 62631-2-1
Dissipation Factor (1 MHz)0.003—IEC 62631-2-1

Table 4 of 4

6 rows
CharacteristicValueUnitMethod
Density1.42g/cm³ISO 1183-1
Water Absorption (After 24h Immersion in Water of 23°C)0.01%ISO 62 (16)
Water Absorption (At Saturation in Water of 23 °C)0.2%—
Wear Rate5µm/kmISO 7148-2 (18)
Dynamic Coefficient of Friction0.2 - 0.35—ISO 7148-2 (18)
Limiting PV (0.1/1 m/s Cylindrical Sleeve Bearings)0.43/0.27Mpa.m/s—

The Omnichem website uses cookies. By continuing to use the site, you consent to their use in accordance with our Privacy Policy and to the collection of analytics.