To catalogue
Wonderloy® PC-510
WONDERLOY® PC-510 is a Polycarbonate + ABS (PC+ABS) product. It can be processed by injection molding and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America.Characteristics include: Flame Rated RoHS Compliant Flame Retardant Halogen Free
Properties
- Physical Form
- Pellets
- Powder
Product families
Plastics — Engineering & Specialty Polymers
- Blends & Alloys
Other characteristics
- Brand
- Wonderloy
- Density
- 1160.0 - 1160.0 kg/m³
- Polymer Name
- PC/ABS Alloy
- Flexural Modulus
- 2600.0 - 2600.0 MPa
- Processing Methods
- Injection Molding
- Color
- Natural
- Flame Rating
- UL 94 V0
- Technology
- Plastics
- Labeling Claims
- Halogen-free
- Additives Included
- Flame Retardant
- Material Features
- Flame Retardant
- Country Availability
- Brazil
- Canada
- China (Mainland)
- Mexico
- USA
- Certifications and Compliance
- RoHS Compliant
- UL 94
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 5
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength at Yield | 49.1 | MPa | ASTM D 638 |
| Stress at break | 45 | MPa | ISO 527 |
| Yield stress | 57 | MPa | ISO 527 |
| Flexural Strength | 78.5 | MPa | ASTM D 790 |
| Flexural modulus, 23° | 2600 | MPa | ISO 178 |
| Flexural Modulus | 2453 | MPa | ASTM D 790 |
| Izod notched impact strength, +23° | 50 | kJ/m2 | ISO 180/1A |
| Izod Impact notched (1/8 in) | 678 | J/m | ASTM D 256 |
Table 2 of 5
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Melt Flow Index - MFI (260°C/2.16 kg) | 20 | g/10 min | ASTM D 1238 |
| Melt Volume Flow Rate - MVR (260°C/2.16 kg) | 23.5 | cm3/10 min | ISO 1133 |
| Mold Shrinkage (MD) | 0.005 | mm/mm | ASTM D 955 |
| Density | 1160 | kg/m3 | ISO 1183 |
Table 3 of 5
7 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Coefficient of Thermal Expansion (MD) | 70 | E-6/K | ASTM D 696 |
| Temperature of deflection under load (1.80 Mpa) | 78 | °C | ISO 75-1/-2 |
| Deflection Temperature Under Load (264 psi) | 77.8 | °C | ASTM D 648 |
| Thickness tested | 1.5 | mm | — |
| Vicat softening temperature | 95 | °C | ISO 306 |
| Vicat Temperature | 93.9 | °C | ASTM D 1525 |
| Burning Behavior 5V at thickness | 5VB | class | IEC 60695-11-20 |
Table 4 of 5
1 row| Characteristic | Value | Method |
|---|---|---|
| Flame rating | V-0 | UL 94 |
Table 5 of 5
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption (24 hr) | 0.4 | % | ASTM D 570 |