Telene® 1750
- Chemical Family
- Olefins
Telene® 1750 technology utilizes ring opening metathesis polymerization (ROMP). Formulations are based on dicyclopentadiene (DCPD) and engineered to produce polydicyclopentadiene polymer (PDCPD), well-known for its robust mechanical properties at low temperatures, its low water absorption, and its radio transparency.
Product families
Applications
- Exterior & Body
- Powertrain & UTH
- Equipment & Parts
Product Families
- Other Thermoset Resins
Other characteristics
- Brand
- Telene Telene
- End Uses
Automotive Bumpers, Automotive Exterior Parts, Automotive Under The Hood, Engine Covers, Fenders
- Polymer Name
- Polydicyclopentadiene (PDCPD)
- Processing Methods
Injection Molding, Reaction Injection Molding (RIM)
- Markets
- Automotive & Transportation
- Industrial
- PACKAGING
- Telene® formulation is supplied in:
- 200 liter drums
- 2,000 liter IBCs
- 20,000 liter ISO containers
- Availability
Telene® offers standard grades based on Molybdenum (x600 family), Tungsten (x700 family) and Ruthenium (x800 family) proprietary catalyst technology.
- Technology
- Plastics
- Material Features
- Corrosion Resistant
- Cost Effective
- Design Flexibility
- Dimensional Stability
- Easier Processing
- Excellent Flexibility
- Excellent Long Term Heat Aging Properties
- Excellent Strength
- Plastics and Elastomers End Uses
- Automotive Bumpers
- Automotive Exterior Parts
- Automotive Under The Hood
- Engine Covers
- Fenders
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
- Reaction Injection Molding (RIM)
Technical data
Table 1 of 2
10 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Specific Gravity | 1.03 | — | ISO 1183 |
| Tensile Modulus | 1850.0 | MPa | ISO 527 |
| Tensile Strength (Yield) | 43.0 | MPa | ISO 527 |
| Elongation (Yield) | 5.0 | % | ISO 527 |
| Flexural Strength | 72.0 | MPa | ISO 178 |
| Flexural Modulus | 1750.0 | MPa | ISO 178 |
| Impact Strength (Notched Izod) (+23°C) | 30.0 | KJ/m2 | ISO 180/A |
| Glass Transition Temperature | 150.0 | °C | — |
| Heat Distortion Temperature (Under 1.8 Mpa Load) | 116.0 | °C | ISO 75/A–Tfe 1,8 |
| Linear Thermal Expansion | 79.10-6 | m/m/°C | ISO 11359 |
Table 2 of 2
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Smoke Time (30°C) | 40 to 80 | Sec | Method 4 |
| Initial Viscosity (30°C) (A & B Component) | 210 - 290 | cp | Brookfield |
| Exotherm Temperature | min. 150 | °C | Method 4 |