To catalogue
Best Plastic Management propylene regrind
- Chemical Family
- PolyolefinsPolypropylenes (PP)
Best Plastic Management Propylene Regrind is used as a casing material for small electrical appliances, molded parts for household appliances and for body parts (bumpers) and molded parts in the interior of motor vehicles. In the construction sector, it is used for pipes, hot water tanks and garden furniture, tubs, plant Containers.
Properties
- Physical Form
- Granules
- Solid
Product families
Applications
Applications
- Consumer Goods — Appliances & Electronics
- Consumer Goods — Furniture
- Consumer Goods — Lawn & Garden
Automotive & Transportation — Automotive
- Chassis & Brake
- Exterior & Body
- Interior
Building & Construction — Building Materials
- Pipes & Plumbing
Industrial — Chemical & Industrial Manufacturing
- Equipment & Parts
Electrical & Electronics — Devices & Assemblies
- Consumer Electronics
Product Families
Plastics — Basic Thermoplastics
- Polyolefins
Other characteristics
- Polymer Name
- Polypropylene (unspecified)
- Processing Methods
- Injection Molding
- Type
- Granulate
- Markets
- Automotive & Transportation
- Building & Construction
- Consumer Goods
- Electrical & Electronics
- Industrial
- Technology
- Plastics
- Labeling Claims
- Environmentally Friendly
- Recycled
- Material Features
- Good Regrind Stability
- Certifications and Compliance
- ISO 50001
- ISO 9001
- Plastics and Elastomers End Uses
- Appliances
- Automotive Bumpers
- Automotive Interior Parts
- Doors
- Furniture
- Pipes
- Shock Absorbers
- Tanks
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 1
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Charpy Impact strength (23°C) | 90.0 | kj/m² | EN ISO 179 |
| Filtration | 6 - 8 | mm | — |
| Charpy notched bar impactstrength (23°C) | 6.0 | kj/m² | EN ISO 179 |
| Density | 0.95 | g/cm³ | EN ISO 55990 |
| Elongation at Yield | min. 50 | % | EN ISO 527 |
| Melt Flow Index (230°C/2.16 kg) | 7.0 | g/10 min | EN ISO 1133 |
| Tensile Modulus | 1400.0 | MPa | EN ISO 527 |
| Tensile Yield Strength | 26.0 | MPa | EN ISO 527 |