To catalogue
Polynil® P50 FL
- Chemical Family
- Polyamides
Nilit POLYNIL® P50 FL is an unreiforced nucleated Polyamide 66 (Nylon 66) for injection molding, UL listed V2.This general pourpose 2.7 viscosity Polyamide 66 resin is designed for fast cycling.
Product families
Plastics — Engineering & Specialty Polymers
- Polyamides
Other characteristics
- Brand
- Polynil
- Polymer Name
- Polyamide 66 (PA 66)
- Flexural Modulus
- 3100.0 - 3100.0 MPa
- Additives Included
- Lubricant (Unspecified), Nucleating Agent
- Lubricant (Unspecified)
- Nucleating Agent
- Processing Methods
- Injection Molding
- Flame Rating
- IEC 60695-11-10 V2
- Technology
- Plastics
- Material Features
- Fast Molding Cycle
- Lubricated
- Nucleated
- Country Availability
- Brazil
- Canada
- China (Mainland)
- Mexico
- USA
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 4
12 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Modulus | 3500 | MPa | ISO 527 |
| Yield stress | 90 | MPa | ISO 527 |
| Yield strain | 5 | % | ISO 527 |
| Strain at break | 30 | % | ISO 527 |
| Flexural modulus, 23° | 3100 | MPa | ISO 178 |
| Charpy notched impact strength (+23°) | 5 | kJ/m2 | ISO 179/1eA |
| Charpy impact strength (+23°) | N | kJ/m2 | ISO 179/1eU |
| Charpy notched impact strength (-30°) | 4.5 | kJ/m2 | ISO 179/1eA |
| Charpy impact strength (-30°) | N | kJ/m2 | ISO 179/1eU |
| Izod notched impact strength, +23° | 4.8 | kJ/m2 | ISO 180/1A |
| Izod notched impact strength | 4.7 | kJ/m2 | ISO 180/1A |
| Temperature | -30 | °C | — |
Table 2 of 4
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Molding shrinkage - normal | 1.2 | % | ISO 294-4, 2577 |
| Molding shrinkage - parallel | 1 | % | ISO 294-4, 2577 |
| Density | 1140 | kg/m3 | ASTM D 792 |
Table 3 of 4
8 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Temperature of deflection under load (1.80 Mpa) | 78 | °C | ISO 75-1/-2 |
| Temperature of deflection under load (0.45 Mpa) | 225 | °C | ISO 75-1/-2 |
| Melting temperature (10°C/min) | 258 | °C | ISO 11357-1/-3 |
| Oxygen index | 28 | % | ISO 4589-1/-2 |
| Thickness tested | 0.8 | mm | — |
| Vicat softening temperature | 240 | °C | ISO 306 |
| Burning Behavior at thickness | V-2 | class | IEC 60695-11-10 |
| Yellow Card available | yes | — | — |
Table 4 of 4
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water absorption | 8.5 | % | Sim. to ISO 62 |