To catalogue

Nylon 6 A1030GFL

Chemical Family
Polyamides

Nylon 6 A1030GFL is a glass fiber-reinforced grade with medium viscosity. It is used for injection molding applications.

Product families

Applications

Applications
  • Consumer Goods — Appliances & Electronics; Consumer Goods — Other Consumer Goods Applications
Automotive & Transportation — Automotive
  • Aftermarket Parts & Components
  • Exterior & Body
  • Interior
  • Powertrain & UTH
Building & Construction — Building Materials
  • Interior Fixtures
  • Other Building Materials
Industrial — Chemical & Industrial Manufacturing
  • Other Industrial Applications
Electrical & Electronics — Devices & Assemblies
  • Consumer Electronics
  • Other Devices & Assemblies
Electrical & Electronics — Parts & Components
  • Other Parts & Components

Product Families

Plastics — Engineering & Specialty Polymers
  • Polyamides

Other characteristics

Brand
Nylon 6
Polymer Name
Polyamide 6 (PA 6)
Fillers Included
Glass Fiber
Processing Methods
Injection Molding
Markets
  • Automotive & Transportation
  • Building & Construction
  • Consumer Goods
  • Electrical & Electronics
  • Industrial
Technology
Plastics
Material Features
Medium Viscosity
Plastics and Elastomers End Uses
  • Appliances
  • Automotive Components
  • Automotive Exterior Parts
  • Automotive Interior Parts
  • Construction Applications
  • Consumer Applications
  • Electrical Parts
  • Electrical/Electronic Applications
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 4

33 rows
CharacteristicValueUnitMethod
Tensile Modulus (Dry)9600MpaISO 527-1 527-2
Charpy Impact Strength (Dry-as-Mold Condition)70kg/m²ISO 179-1
Tensile Modulus (Condition)6000MpaISO 527-1 527-2
Tensile Strain at Break (Dry)3.1%ISO 527-1 527-2
Charpy Notched Impact Strength (Dry-as-Mold Condition)11kg/m²ISO 179-1
Tensile Strain at Break (Condition)5.3——
Flexural Modulus (Dry-as-Mold Condition)8200MpaISO 178
Charpy Impact Strength (Conditioned to Equilibirium at 23°C, 50%RH)85kg/m²ISO 179-1
Charpy Impact Strength (Conditioned)85kg/m²ISO 179-1
Flexural Strength (Dry-as-Mold Condition)250MpaISO 178
Charpy Impact Strength (Dry)70kg/m²ISO 179-1
Charpy Notched Impact Strength (Conditioned to Equilibirium at 23°C, 50%RH)19kg/m²ISO 179-1

Table 2 of 4

3 rows
CharacteristicValueUnitMethod
Coefficient of Linear Thermal Expansion3.110⁻⁵/°CISO 11359-2
Deflection Temperature (Under load 0.45MPa)217°CISO 75-2
Deflection Temperature (Under load 1.8MPa)203°CISO 75-1

Table 3 of 4

6 rows
CharacteristicValueUnitMethod
Mold Shrinkage (Thickness : 3.2mm, Flow)0.2%—
Mold Shrinkage (Thickness : 3.2mm, Transverse)0.7%—
Water Absorption (23°C in Water 24H)1.3%ISO 62
Water Absorption (23°C, 50% RH Equilibirium)2%ISO 62
Flammability (mmt HB)0.75—UL-94
Density1.36g/cm³ISO 1183

Table 4 of 4

17 rows
CharacteristicValueUnitMethod
Dielectric Constant (106Hz, Conditioned)3—IEC 60250
Dielectric Constant (106Hz, Dry)3.3—IEC 60250
Dielectric Constant (Conditioned to Equilibirium at 23°C, 50%RH)3.610⁶ HzIEC 60250
Comparative Tracking Index550—IEC 60112
Dissipation Factor (106Hz, Conditioned)0.12—IEC 60250
Dissipation Factor (106Hz, Dry)0.022—IEC 60250
Dissipation Factor (Conditioned to Equilibirium at 23°C, 50%RH)0.1210⁶ HzIEC 60250
Electric Strength (Thickness:1mm, Conditioned to Equilibirium at 23°C, 50%RH)44MV/mIEC 60243-1
Dielectric Constant (Dry-as-Mold Condition)3.310⁶ HzIEC 60250
Electric Strength (Thickness:1mm, Conditioned)44MV/mIEC 60243-1
Dissipation Factor (Dry-as-Mold Condition)0.02210⁶ HzIEC 60250
Electric Strength (Thickness:1mm, Dry)42MV/mIEC 60243-1