Silopren™ LSR 2641
- Chemical Family
- Silicones
Silopren™ LSR 2641 TP 3730 is a two-component liquid silicone rubber for injection molding processes.Silopren™ LSR 2641 TP 3730 shows in comparison to Silopren™ LSR 2640 as non post-cure grade (NPC grade)a lower compression set after vulcanisation.Key Features and Benefits Vulcanisates consisting of Silopren™ LSR 2641 TP 3730 are distinguished by the following properties: non post-cure high reactivity excellent thermal stability high stability and flexibility at low temperatures good rubber-like properties, high tear resistance long service life at dynamic stress high stability to ozone and ultraviolet light outstanding resistance to aging, excellent dielectric behavior over a wide range of temperatures, not readily combustible, does not melt or drip easy pigmentable with the LSR Color Pastes Potential ApplicationsBecause of the outstanding properties Silopren™ LSR 2641 TP 3730 is particularly suitable for the following elastomeric articles: sealing elements, O-rings, stoppers, diaphragms, keypads, bellows,vibration dampers, switch cover, spark plug boots, cable connectors s.o.
Properties
- Physical Form
- Liquid
Product families
Applications
- Connectors
Product Families
- Silicone Elastomers
Other characteristics
- Brand
- Silopren
- End Uses
- Connectors
- Features
Good Colorability, Good Stability, Good Tear Strength, Good Thermal Stability, High Reactivity, Low Temperature Flexibility, Ozone Resistant, UV Resistant, Vibration Damping
- Polymer Name
- Liquid Silicone Rubber (LSR)
- Tear Strength
- 35.0 - 35.0 kN/m
- Processing Methods
- Injection Molding
- Markets
- Electrical & Electronics
- Appearance
- Translucent
- Technology
- Elastomers
- Material Features
- Good Colorability
- Good Stability
- Good Tear Strength
- Good Thermal Stability
- High Reactivity
- Low Temperature Flexibility
- Ozone Resistant
- UV Resistant
- Country Availability
- Brazil
- Canada
- China (Mainland)
- Mexico
- USA
- Plastics and Elastomers End Uses
- Connectors
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 2
4 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 9 | MPa | ISO 527 |
| Hardness | 40 | Shore A | ISO 7619-1 |
| Strain at break | 700 | % | ISO 37 |
| Tear Strength | 35 | kN/m | ASTM D 624 |
Table 2 of 2
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Density | 1110 | kg/m3 | ISO 1183 |