Amorvon® WL-30
- Chemical Family
- FluoropolymersPolyphenylene Sulfide (PPS)
Product families
Applications
Automotive & Transportation — Automotive
- Other Automotive Applications
- Powertrain & UTH
Building & Construction — Building Materials
- Structural Components
Industrial — Chemical & Industrial Manufacturing
- Equipment & Parts
- Other Industrial Applications
Electrical & Electronics — Devices & Assemblies
- Automotive Electronics
- Other Devices & Assemblies
Electrical & Electronics — Parts & Components
- Other Parts & Components
Product Families
Plastics — Engineering & Specialty Polymers
- Blends & Alloys
Other characteristics
- Brand
- Amorvon
- Density
- 1680.0 - 1680.0 kg/m³
- Polymer Name
- PPS/PTFE Alloy
- Flexural Modulus
- 9000.0 - 9000.0 MPa
- Tensile Strength
- 150.0 - 150.0 MPa
- Processing Methods
- Injection Molding
- Color
- Black
- Markets
- Automotive & Transportation
- Building & Construction
- Electrical & Electronics
- Industrial
- Flame Rating
- UL 94 V0
- Technology
- Plastics
- Fillers Included
- Glass Fiber
- Additives Included
- Lubricant (Unspecified)
- Material Features
- Tribological Modified
- Country Availability
- Canada
- China (Mainland)
- USA
- Certifications and Compliance
- UL 94
- Plastics and Elastomers End Uses
- Bearings
- Gears
- Industrial Applications
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 6
9 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Tensile Strength | 150 | MPa | ISO 527 |
| Elongation at Break | 1.6 | % | ASTM D 638 |
| Tensile Modulus | 10000 | MPa | ISO 527 |
| Flexural Strength | 200 | MPa | ASTM D 790 |
| Flexural Modulus | 9000 | MPa | ASTM D790 |
| Izod Impact notched (1/8 in) | 60 | J/m | ASTM D 256 |
| Izod Impact unnotched (1/8 in) | 350 | J/m | ASTM D 256 |
| Rockwell Hardness | 118 | Scale R | ASTM D 785 |
| Compressive Strength | 170 | MPa | ASTM D 695 |
Table 2 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Mold Shrinkage (MD) | 0.0025 | mm/mm | ASTM D 955 |
| Mold Shrinkage (TD) | 0.01 | mm/mm | ASTM D 955 |
| Density | 1680 | kg/m3 | ISO 1183 |
Table 3 of 6
3 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Coefficient of Thermal Expansion (MD) | 23 | E-6/K | ASTM D 696 |
| Deflection Temperature Under Load (264 psi) | 230 | °C | ASTM D 648 |
| Thickness tested | 0.8 | mm | — |
Table 4 of 6
5 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Dissipation Factor (1 MHz) | 0.002 | — | ASTM D 150 |
| Dielectric Strength (Short Time) | 16 | kV/mm | ASTM D 149 |
| Dielectric Constant (1 MHz) | 4 | — | ASTM D 150 |
| Arc Resistance | 120 | s | ASTM D 495 |
| Volume Resistivity | min. 1E15 | ohm.m | ASTM D 257 |
Table 5 of 6
1 row| Characteristic | Value | Method |
|---|---|---|
| Flame rating | V-0 | UL 94 |
Table 6 of 6
1 row| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Water Absorption (24 hr) | 0.05 | % | ASTM D 570 |