To catalogue
EVERLON® TC-63
- Chemical Family
- Styrenics
EVERLON® TC-63 is a High quality of strength and transparent: including crystal-clean grade and is based on SEBS, which is great at flexibility and elongation rate.
Product families
Applications
Healthcare & Pharma — Medical
- Disposable Nonwovens
- Medical Devices & Assemblies
- Other Medical Applications
Printing & Packaging — Packaging
- Healthcare Packaging
Food & Nutrition — Processing & Packaging
- Food & Beverage Manufacturing
Product Families
Elastomers — Thermoplastic Elastomers
- Styrenic Thermoplastic Elastomers (TPE-S)
Other characteristics
- Brand
- EVERLON
- Polymer Name
- Styrene Ethylene Butylene Styrene (SEBS)
- Tear Strength
- 41.16 - 41.16 kN/m
- Strain at Break
- 600.0 - 600.0 %
- Processing Methods
- Injection Molding
- Usage
Comply with the FDA standard, great to use on the medical instruments and food instruments.
- Color
- Transparent
- Markets
- Food & Nutrition
- Healthcare & Pharma
- Printing & Packaging
- Technology
- Elastomers
- Labeling Claims
- Food Contact Acceptable
- Material Features
- Consistent High Quality
- Food Contact Acceptable
- Good Elongation
- Good Flexibility
- Good Strength
- High Clarity
- Certifications and Compliance
- FDA Compliant
- ISO 9001
- UL Certified
- Plastics and Elastomers End Uses
- Medical Devices
- Medical Reusable Masks
- Medical/Healthcare Applications
- Pharmaceutical Stoppers
- Tubing
- Plastics and Elastomers Functions
- Resin
- Plastics and Elastomers Processing Methods
- Injection Molding
Technical data
Table 1 of 1
6 rows| Characteristic | Value | Unit | Method |
|---|---|---|---|
| Hardness | 60.0 | Shore A | ASTM D2240 |
| Specific Gravity | 0.9 | — | ASTM D792 |
| Tensile Strength | 65.0 | kg/cm2 | ASTM D412 |
| Elongational Break | 600.0 | % | ASTM D412 |
| Tear Strength | 42.0 | kg/cm | ASTM D624 |
| Brittle Temperature | -40.0 | — | ASTM D746 |