ROMILOY® 5240 GF20

Chemical Family
PolyestersStyrenics

ROMILOY® 5240 GF20 is ASA/PBT, injection molding grade, 20% glass fiber reinforced, high dimensional stability, high surface quality.

Properties

Physical Form
  • Pellets
  • Solid

Product families

Applications

Applications
  • Automotive & Transportation — Other Automotive & Transportation Applications; Consumer Goods — Other Consumer Goods Applications; Electrical & Electronics — Other Electrical & Electronics Applications; Healthcare & Pharma — Other Healthcare & Pharma Applications
Automotive & Transportation — Automotive
  • Electrical & Electronic Systems
  • Other Automotive Applications
Building & Construction — Building Envelope & Roofing
  • Other Building Envelope & Roofing Applications
Building & Construction — Building Materials
  • Other Building Materials

Product Families

Plastics — Engineering & Specialty Polymers
  • Blends & Alloys

Other characteristics

Brand
ROMILOY
Polymer Name
PBT/ASA Alloy
Processing Methods
Injection Molding
Markets
  • Automotive & Transportation
  • Building & Construction
  • Consumer Goods
  • Electrical & Electronics
  • Healthcare & Pharma
Technology
Plastics
Fillers Included
Glass Fiber
Material Features
  • Dimensional Stability
  • Superior Surface Quality
Certifications and Compliance
  • Halal
  • Kosher
Plastics and Elastomers Functions
Resin
Plastics and Elastomers Processing Methods
Injection Molding

Technical data

Table 1 of 3

2 rows
CharacteristicValueUnitMethod
Water Absorption (23 °C, 50 % RH, 24 h)6.5kJ/m²DIN EN ISO 179/1eA
Density (23 °C, 50 % RH)150MPaDIN EN ISO 1133

Table 2 of 3

7 rows
CharacteristicValueUnitMethod
Elongation at Break (50 mm/min 23 °C)1.38g/cm³DIN EN ISO 1183
Impact Strength (Charpy)6.4%DIN EN ISO 527
Impact Strength (Charpy)5600MPaDIN EN ISO 178
Notched Impact Strength (Charpy at 80 x 10 x 4 23 °C)38g/10 minDIN EN ISO 1133
Notched Impact Strength (Charpy at 80 x 10 x 4 23 °C)158°CDIN EN ISO 306
Tensile Modulus (1 mm/min 23 °C)6600MPaDIN EN ISO 527
Tensile Strength (50 mm/min 23 °C)95MPaDIN EN ISO 527

Table 3 of 3

5 rows
CharacteristicValueUnitMethod
Flammability (own test)HB—UL94
Heat deflection temperature (HDT/A)5.5kJ/m²DIN EN ISO 179/1eA
Melt Mass-Flow Rate (MFR)42kJ/m²DIN EN ISO 179/1eU
Processing Shrinkage (220 °C, 10 kg)0.3 0.6%DIN EN ISO 294-4
Vicat Softening Temperature (B 50)45kJ/m²DIN EN ISO 179/1eU